CC BY-NC-ND 4.0 · Eur J Dent 2019; 13(03): 470-477
DOI: 10.1055/s-0039-1693524
Review Article
Dental Investigation Society

Modifications of Glass Ionomer Cement Powder by Addition of Recently Fabricated Nano-Fillers and Their Effect on the Properties: A Review

1   School of Dental Sciences, Universiti Sains Malaysia, Kubang Kerian, Kelantan, Malaysia
,
1   School of Dental Sciences, Universiti Sains Malaysia, Kubang Kerian, Kelantan, Malaysia
,
1   School of Dental Sciences, Universiti Sains Malaysia, Kubang Kerian, Kelantan, Malaysia
,
1   School of Dental Sciences, Universiti Sains Malaysia, Kubang Kerian, Kelantan, Malaysia
,
1   School of Dental Sciences, Universiti Sains Malaysia, Kubang Kerian, Kelantan, Malaysia
,
2   Department of Restorative Dentistry, Lincoln University College, Selangor, Malaysia
› Author Affiliations
Funding This work was supported by the Malaysian Ministry of Higher Education under Fundamental Research Grant Scheme (FRGS/203/PPSG/6171173).
Further Information

Publication History

Publication Date:
07 July 2019 (online)

Abstract

The aim of this article is to provide a brief insight regarding the recent studies and their recommendations related to the modifications to glass ionomer cement (GIC) powder in order to improve their properties. An electronic search of publications was made from the year 2000 to 2018. The databases included in the current study were EBSCOhost, PubMed, and ScienceDirect. The inclusion criteria for the current study include publication with abstract or full-text articles, original research, reviews or systematic reviews, in vitro, and in vivo studies that were written in English language. Among these only articles published in peer-reviewed journals were included. Articles published in other languages, with no available abstract and related to other nondentistry fields, were excluded. A detailed review of the recent materials used as a filler phase in GIC powder has revealed that not all modifications produce beneficial results. Recent work has demonstrated that modification of GIC powder with nano-particles has many beneficial effects on the properties of the material. This is due to the increase in surface area and surface energy, along with better particle distribution of the nano-particle. Therefore, more focus should be given on nano-particle having greater chemical affinity for GIC matrix as well as the tooth structure that will enhance the physicochemical properties of GIC.

 
  • References

  • 1 Wilson AD, Kent BE. A new translucent cement for dentistry. The glass ionomer cement. Br Dent J 1972; 132 (04) 133-135
  • 2 Najeeb S, Khurshid Z, Zafar MS. et al. Modifications in glass ionomer cements: nano-sized fillers and bioactive nanoceramics. Int J Mol Sci 2016; 17 (07) E1134
  • 3 Ching HS, Luddin N, Kannan TP, Ab Rahman I, Abdul Ghani NR. Modification of glass ionomer cements on their physical-mechanical and antimicrobial properties. J Esthet Restor Dent 2018; 30 (06) 557-571
  • 4 Berg JH, Croll TP. Glass ionomer restorative cement systems: an update. Pediatr Dent 2015; 37 (02) 116-124
  • 5 Elsaka SE, Hamouda IM, Swain MV. Titanium dioxide nanoparticles addition to a conventional glass-ionomer restorative: influence on physical and antibacterial properties. J Dent 2011; 39 (09) 589-598
  • 6 Kobayashi M, Kon M, Asaoka K, Miyai K. Strengthening of glass-ionomer cement by compounding short glass-fibers. J Dent Res 2000; 79: 539-539
  • 7 Sajjad A, Bakar WZ, Mohamad D, Kannan T. Various recent reinforcement phase incorporations and modifications in glass ionomer powder compositions: a comprehensive review. J Int Oral Health 2018; 10 (04) 161-167
  • 8 Moshaverinia A, Ansari S, Moshaverinia M, Roohpour N, Darr JA, Rehman I. Effects of incorporation of hydroxyapatite and fluoroapatite nanobioceramics into conventional glass ionomer cements (GIC). Acta Biomater 2008; 4 (02) 432-440
  • 9 Paiva L, Fidalgo TKS, da Costa LP. et al. Antibacterial properties and compressive strength of new one-step preparation silver nanoparticles in glass ionomer cements (NanoAg-GIC). J Dent 2018; 69: 102-109
  • 10 Garcia-Contreras R, Scougall-Vilchis RJ, Contreras-Bulnes R, Sakagami H, Morales-Luckie RA, Nakajima H. Mechanical, antibacterial and bond strength properties of nano-titanium-enriched glass ionomer cement. J Appl Oral Sci 2015; 23 (03) 321-328
  • 11 Yli-Urpo H, Lassila LVJ, Närhi T, Vallittu PK. Compressive strength and surface characterization of glass ionomer cements modified by particles of bioactive glass. Dent Mater 2005; 21 (03) 201-209
  • 12 Hench LL, Xynos ID, Polak JM. Bioactive glasses for in situ tissue regeneration. J Biomater Sci Polym Ed 2004; 15 (04) 543-562
  • 13 Farooq I, Moheet IA, Alshwaimi E. Cavity cutting efficiency of a Bioglass TM and alumina powder combination utilized in an air abrasion system. Bull Mater Sci 2016; 39 (06) 1531-1536
  • 14 Yli-Urpo H, Närhi T, Söderling E. Antimicrobial effects of glass ionomer cements containing bioactive glass (S53P4) on oral micro-organisms in vitro. Acta Odontol Scand 2003; 61 (04) 241-246
  • 15 De Caluwé T, Vercruysse CWJ, Declercq HA, Schaubroeck D, Verbeeck RMH, Martens LC. Bioactivity and biocompatibility of two fluoride containing bioactive glasses for dental applications. Dent Mater 2016; 32 (11) 1414-1428
  • 16 De Caluwé T, Vercruysse CWJ, Ladik I. et al. Addition of bioactive glass to glass ionomer cements: effect on the physico-chemical properties and biocompatibility. Dent Mater 2017; 33 (04) e186-e203
  • 17 Kobayashi M, Kon M, Miyai K, Asaoka K. Strengthening of glass-ionomer cement by compounding short fibres with CaO-P2O5-SiO2-Al2O3 glass. Biomaterials 2000; 21 (20) 2051-2058
  • 18 Kawano F, Kon M, Kobayashi M, Miyai K. Reinforcement effect of short glass fibers with CaO- P(2)O(5) -SiO(2) -Al(2)O(3) glass on strength of glass-ionomer cement. J Dent 2001; 29 (05) 377-380
  • 19 Lohbauer U, Frankenberger R, Clare A, Petschelt A, Greil P. Toughening of dental glass ionomer cements with reactive glass fibres. Biomaterials 2004; 25 (22) 5217-5225
  • 20 Lohbauer U, Walker J, Nikolaenko S. et al. Reactive fibre reinforced glass ionomer cements. Biomaterials 2003; 24 (17) 2901-2907
  • 21 Garoushi S, Vallittu P, Lassila L. Hollow glass fibers in reinforcing glass ionomer cements. Dent Mater 2017; 33 (02) e86-e93
  • 22 Farooq I, Moheet IA, AlShwaimi E. In vitro dentin tubule occlusion and remineralization competence of various toothpastes. Arch Oral Biol 2015; 60 (09) 1246-1253
  • 23 Lucas ME, Arita K, Nishino M. Strengthening a conventional glass ionomer cement using hydroxyapatite. J Dent Res 2001; 80: 711
  • 24 Lucas ME, Arita K, Nishino M. Toughness, bonding and fluoride-release properties of hydroxyapatite-added glass ionomer cement. Biomaterials 2003; 24 (21) 3787-3794
  • 25 Gu YW, Yap AU, Cheang P, Khor KA. Effects of incorporation of HA/ZrO(2) into glass ionomer cement (GIC). Biomaterials 2005; 26 (07) 713-720
  • 26 Yap AUJ, Pek YS, Kumar RA, Cheang P, Khor KA. Experimental studies on a new bioactive material: HAIonomer cements. Biomaterials 2002; 23 (03) 955-962
  • 27 Huang S, Gao S, Cheng L, Yu H. Remineralization potential of nano-hydroxyapatite on initial enamel lesions: an in vitro study. Caries Res 2011; 45 (05) 460-468
  • 28 Huang SB, Gao SS, Yu HY. Effect of nano-hydroxyapatite concentration on remineralization of initial enamel lesion in vitro. Biomed Mater 2009; 4 (03) 34-104
  • 29 Lee JJ, Lee YK, Choi BJ. et al. Physical properties of resin-reinforced glass ionomer cement modified with micro and nano-hydroxyapatite. J Nanosci Nanotechnol 2010; 10 (08) 5270-5276
  • 30 Tjandrawinata R, Irie M, Suzuki K. Marginal gap formation and fluoride release of resin-modified glass-ionomer cement: effect of silanized spherical silica filler addition. Dent Mater J 2004; 23 (03) 305-313
  • 31 Hatanaka K, Irie M, Tjandrawinata R, Suzuki K. Effect of spherical silica filler addition on immediate interfacial gap-formation in Class V cavity and mechanical properties of resin-modified glass-ionomer cement. Dent Mater J 2006; 25 (03) 415-422
  • 32 Shiekh RA, Ab Rahman I, Masudi SM, Luddin N. Modification of glass ionomer cement by incorporating hydroxyapatite-silica nano-powder composite: Sol-gel synthesis and characterization. Ceram Int 2014; 40 (02) 3165-3170
  • 33 Yan H, Yang H, Li K, Yu J, Huang C. Effects of chlorhexidine-encapsulated mesoporous silica nanoparticles on the anti-biofilm and mechanical properties of glass ionomer cement. Molecules 2017; 22 (07) 1225
  • 34 Felemban NH, Ebrahim MI. Effects of adding silica particles on certain properties of resin-modified glass-ionomer cement. Eur J Dent 2016; 10 (02) 225-229
  • 35 Rahman IA, Masudi SAM, Luddin N, Shiekh RA. One-pot synthesis of hydroxyapatite–silica nanopowder composite for hardness enhancement of glass ionomer cement (GIC). Bull Mater Sci 2014; 37 (02) 213-219
  • 36 Moheet IA, Luddin N, Ab Rahman I, Masudi SaM, Kannan TP, Abd Ghani NR. Evaluation of mechanical properties and bond strength of nano-hydroxyapatite-silica added glass ionomer cement. Ceram Int 2018; 44 (08) 9899-9906
  • 37 Elie ED, Maha A-G. The zirconia restoration properties: a versatile restorative material. Dentistry. 2014;4(4)
  • 38 Rajabzadeh G, Salehi S, Nemati A, Tavakoli R, Solati Hashjin M. Enhancing glass ionomer cement features by using the HA/YSZ nanocomposite: a feed forward neural network modelling. J Mech Behav Biomed Mater 2014; 29: 317-327
  • 39 Anusha Thampi VV, Prabhu M, Kavitha K. et al. Hydroxyapatite, alumina/zirconia, and nanobioactive glass cement for tooth-restoring applications. Ceram Int 2014; 40 (9, Part A) 14355-14365
  • 40 Ab Rahman I, Ghazali NAM, Bakar WZ, Masudi SM. Modification of glass ionomer cement by incorporating nanozirconia-hydroxyapatite-silica nano-powder composite by the one-pot technique for hardness and aesthetics improvement. Ceram Int 2017; 43 (16) 13247-13253
  • 41 Xie D, Feng D, Chung I-D, Eberhardt AW. A hybrid zinc-calcium-silicate polyalkenoate bone cement. Biomaterials 2003; 24 (16) 2749-2757
  • 42 Boyd D, Towler MR. The processing, mechanical properties and bioactivity of zinc based glass ionomer cements. J Mater Sci Mater Med 2005; 16 (09) 843-850
  • 43 Dickey BT, Kehoe S, Boyd D. Novel adaptations to zinc-silicate glass polyalkenoate cements: the unexpected influences of germanium based glasses on handling characteristics and mechanical properties. J Mech Behav Biomed Mater 2013; 23: 8-21
  • 44 Khader BA, Peel SAF, Towler MR. An injectable glass polyalkenoate cement engineered for fracture fixation and stabilization. J Funct Biomater 2017; 8 (03) E25
  • 45 Leitune VC, Collares FM, Takimi A. et al. Niobium pentoxide as a novel filler for dental adhesive resin. J Dent 2013; 41 (02) 106-113
  • 46 Bertolini MJ, Palma-Dibb RG, Zaghete MA, Gimenes R. Evaluation of glass ionomer cements properties obtained from niobium silicate glasses prepared by chemical process. J Non-Cryst Solids 2005; 351 6-7 466-471
  • 47 Garcia IM, Leitune VCB, Balbinot GS, Samuel SMW, Collares FM. Influence of niobium pentoxide addition on the properties of glass ionomer cements. Acta Biomater Odontol Scand 2016; 2 (01) 138-143
  • 48 Prentice LH, Tyas MJ, Burrow MF. The effect of ytterbium fluoride and barium sulphate nanoparticles on the reactivity and strength of a glass-ionomer cement. Dent Mater 2006; 22 (08) 746-751
  • 49 Al Zraikat H, Palamara JE, Messer HH, Burrow MF, Reynolds EC. The incorporation of casein phosphopeptide-amorphous calcium phosphate into a glass ionomer cement. Dent Mater 2011; 27 (03) 235-243
  • 50 Oshiro M, Yamaguchi K, Takamizawa T. et al. Effect of CPP-ACP paste on tooth mineralization: an FE-SEM study. J Oral Sci 2007; 49 (02) 115-120
  • 51 Farooq I, Moheet IA, Imran Z, Farooq U. A review of novel dental caries preventive material: casein phosphopeptide–amorphous calcium phosphate (CPP–ACP) complex. King Saud University Journal Of Dental Sciences 2013; 4 (02) 47-51
  • 52 Zalizniak I, Palamara JE, Wong RH, Cochrane NJ, Burrow MF, Reynolds EC. Ion release and physical properties of CPP-ACP modified GIC in acid solutions. J Dent 2013; 41 (05) 449-454
  • 53 Ni S, Chou L, Chang J. Preparation and characterization of forsterite (Mg2SiO4) bioceramics. Ceram Int 2007; 33 (01) 83-88
  • 54 Sayyedan FS, Fathi MH, Edris H, Doostmohammadi A, Mortazavi V, Hanifi A. Effect of forsterite nanoparticles on mechanical properties of glass ionomer cements. Ceram Int 2014; 407 Part B 10743-10748
  • 55 Sayyedan FS, Fathi M, Edris H, Doostmohammadi A, Mortazavi V, Shirani F. Fluoride release and bioactivity evaluation of glass ionomer: forsterite nanocomposite. Dent Res J (Isfahan) 2013; 10 (04) 452-459
  • 56 Kim DA, Abo-Mosallam HA, Lee HY, Kim GR, Kim HW, Lee H-H. Development of a novel aluminum-free glass ionomer cement based on magnesium/strontium-silicate glasses. Mater Sci Eng C 2014; 42: 665-671
  • 57 Brauer DS, Karpukhina N, Kedia G. et al. Bactericidal strontium-releasing injectable bone cements based on bioactive glasses. J R Soc Interface 2013; 10 (78) 20120647
  • 58 Sinha Ray S, Okamoto M. Polymer/layered silicate nanocomposites: a review from preparation to processing. Prog Polym Sci 2003; 28 (11) 1539-1641
  • 59 Dowling AH, Stamboulis A, Fleming GJP. The influence of montmorillonite clay reinforcement on the performance of a glass ionomer restorative. J Dent 2006; 34 (10) 802-810
  • 60 Fareed MA, Stamboulis A. Effect of nanoclay dispersion on the properties of a commercial glass ionomer cement. Int J Biomater 2014; 2014: 685389
  • 61 Fareed MA, Stamboulis A. Nanoclay-reinforced glass-ionomer cements: in vitro wear evaluation and comparison by two wear-test methods. Dent J (Basel) 2017; 5 (04) 28
  • 62 Silva RM, Pereira FV, Mota FA, Watanabe E, Soares SM, Santos MH. Dental glass ionomer cement reinforced by cellulose microfibers and cellulose nanocrystals. Mater Sci Eng C 2016; 58: 389-395
  • 63 Sun J, Xu y, Zhu B. et al. Synergistic effects of titanium dioxide and cellulose on the properties of glassionomer cement. Dent Mater 2019; 38 (01) 41-51
  • 64 Sun L, Yan Z, Duan Y, Zhang J, Liu B. Improvement of the mechanical, tribological and antibacterial properties of glass ionomer cements by fluorinated graphene. Dent Mater 2018; 34 (06) e115-e127